← Raku · basics and all recipes
Illustration of the expected effect: Naked raku: resist slip
AI illustration of the expected effect. Not a fired result.

Naked raku · resist slipNaked rakuIntermediate

Naked raku: resist slip

About 930–980 °C (1700–1800 °F)

A layer that peels off after the firing. Underneath, the clay stays pale where the glaze protected it and turns black where smoke got through the cracks: fine, ink-like lines.

Recipe

Base

Fireclay50
EPK kaolinor any white kaolin30
Alumina hydrateor calcined alumina20
Total100

Firing and reduction

Best on burnished or terra-sigillata pieces. Apply a medium coat, let it dry, then cover it with the sacrificial glaze. More alumina makes it release more easily. After reduction, wash and scrub: slip and glaze come off together.

A formulated starting point. We have not fired it in our studio with these exact materials yet, so test it on a tile before a real piece.

Raku is decorative. The body stays porous and the glazes are unstable on purpose. Never use a raku piece for food or drink. Fire outdoors, with heat gloves and a face shield.